[time-nuts] quartz / liquid nitrogen
Mark Sims
holrum at hotmail.com
Tue Apr 3 01:26:17 EDT 2018
And you want your semiconductors to be in ceramic/lided packages with the bond wires flapping in free air. Bond wires embedded in epoxy like to break... don't ask how I found this out ;-) ... it brings back bad memories... and makes bad memories... Quantum chips have very elaborate/specialized bonding to survive liquid helium... even with that, thermal cycling still breaks them.